High refractoriness
Anti-acid
Anti-alkaline slag
High refractoriness
Anti-acid
Anti-alkaline slag
High alumina bricks for carbon roasting furnaces are aluminum silicate refractory bricks with Al₂O₃ content greater than 48%. The production process is similar to clay refractory bricks. According to different grades of bauxite clinker, different quality requirements, and formula binders The selection and distribution of appropriate proportions are formed by pressing bricks and then calcined.
Project | ||||
---|---|---|---|---|
AL2O3 (%) | 75 | 65 | 55 | 85 |
Fe203 (%) | 2.5 | 2.5 | 2.6 | 2 |
Bulk density g/cm³ | 2.5 | 2.4 | 2.3 | 2.6 |
Normal temperature compressive strength MPa | 70 | 60 | 50 | 80 |
Load softening temperature ℃ | 1510 | 1460 | 1420 | 1550 |
Refractoriness ℃ | 1790 | 1770 | 1770 | 1790 |
Apparent porosity (%) | 22 | 23 | 24 | 21 |
Line rate of change (%) | -0.3 | -0.4 | -0.4 | -0.2 |
High alumina bricks for carbon roasting furnace are mainly used in the bottom, side wall, flue wall, transverse wall, furnace roof and flue of carbon roasting furnace.